Sep 27th, 2011, 09:46 PM
Flagg- It's good to meet a clay expert.
This is oil-based, with several grades of microcrystalline as the binder. Thrash0, fuck off. The grease that makes the more brittle waxes stick to the marble dust and talc is petroleum jelly and the oil is mineral oil.
The heating element is either a heat gun or a stove burner; I only recently started using a heat gun because it was faster and I have not observed any health issues aside from a burning pain in my stomach and the constant need to urinate.
The two pans which make up the double boiler do not come in contact with food, except I do put wads of chewing gum in there sometimes and I've used them as an ashtray.
...this is the chat thread, don't expect a straight answer. I think it belongs in Art Shit, though.